Cause countermeasure

picture

(1) The true sand rate is low, and the sand contains too much stone: increase the sand rate and increase the true sand content.
(2) Less fine particle content in sand: increase the amount of admixture and make necessary supplements.
(3) Unreasonable stone grading, single particle size: increase sand rate 2-5%.
(4) Large bleeding rate of cement and admixture: replace cement and admixture; Thickening components in admixtures.
(5) Coarse fly ash particles, high carbon content: replace fly ash.
(6) Low strength grade concrete: use air entrainment agent or increase the amount of cementing material.
(7) High-strength grade concrete: reduce the amount of admixtures or reduce the slow-setting components in the admixtures.
(8) There is water in the tank car: reverse the mixing tank before loading ash, and discharge the water.
(9) Unknown reason: change the admixture formula or take the above comprehensive measures.

Send Inquiry
Contact Us
    • Mobile:+86 15589354098
    • Tel:+86 533 3146528
    • Email:sales@zhuoxingchem.com
    • Email:sales02@zhuoxingchem.com
    • Email:sales03@zhuoxingchem.com
    •  
    • Add: Block B, Yunlong International, Zhangdian District, Zibo City, Shandong Province, China.