Second, clay meets cement particles or polycarboxylic superplasticizer to form hydration, swelling hydration film, resulting in cement particles can not adsorb admixtures, resulting in reduced dispersion;
Third, when clay meets carboxylic acid superplasticizer, the negative effect of clay increases. The large amount of adsorption of carboxylic acid on clay surface causes cement particles and clay surface to compete for the adsorption of carboxylic acid superplasticizer. The adsorption capacity of clay is greater than that of cement particles, resulting in poor fluidity of concrete
Among the three mechanisms, the third is generally considered to be a practical mechanism. The first mechanism can occur at high temperature, and the second mechanism has no obvious effect through the addition of KCl solution. Through the analysis of concrete application of the third kind of mechanism, it is found that the adsorption capacity of clay to polycarboxylic superplasticizer is very large. The adsorption capacity increases linearly with the increase of clay percentage, and the maximum adsorption capacity is stable at 80% of the total amount of polycarboxylate superplasticizer. When the mud content of sand is 3%, the effect of polycarboxylic acid superplasticizer is obvious. When the mud content reaches 7%, the contribution value of 30% of carboxylic acid superplasticizer is absorbed by clay, which greatly affects the fluidity of concrete.