There are bubbles on the surface after hardening. Reason: in order to facilitate the construction, the dosage of water-reducing agent is increased.Treatment: strictly according to the proportion of construction, improve the construction process, strengthen the construction management.Concrete setting and hardening slowly, the reason: the amount of water reducing agent or curing temperature is not enough.Treatment: strictly according to the proportion of construction, extend the maintenance time.Concrete slump and design values are obviously different. The reason is that two kinds of admixtures are used together and are incompatible.Treatment method: do compatibility test before use, adjust mixing proportion.
The concrete prepared with polycarboxylate superplasticizer can reach the standard of clear concrete with uniform bright color, compact surface and few bubbles.